unrealalex (www.ambrotype.ru)
Mythbuster [wet-plate collodion negative]
To find a truth I made a simple test. I had hypo and Amm. Thio and I want to understand are there any difference in picture using those fixers.
So I made an exposure then develop and then cut a glass in two parts.
One part I fixed in Hypo and another in Amm. Thio... try to find 10 difference in them :)))
*For sure I scan two pieces by one pass by putting them together on scanner glass.
Fixing time (until all whites is gone):
Hypo: 2 minutes
Amm thio: 30-40 seconds
Collodion: "Same Day Extra Dry"
Potassium Iodide + Potassium Bromide
Mythbuster [wet-plate collodion negative]
To find a truth I made a simple test. I had hypo and Amm. Thio and I want to understand are there any difference in picture using those fixers.
So I made an exposure then develop and then cut a glass in two parts.
One part I fixed in Hypo and another in Amm. Thio... try to find 10 difference in them :)))
*For sure I scan two pieces by one pass by putting them together on scanner glass.
Fixing time (until all whites is gone):
Hypo: 2 minutes
Amm thio: 30-40 seconds
Collodion: "Same Day Extra Dry"
Potassium Iodide + Potassium Bromide