Pyrocat HD 04
TESTS of KENTMERE 400 120 size in home-made PYROCAT HD Staining Developer . I rated film 320 ASA and gave 17 mins @ 20oC -- there seems to be a High FOG LEVEL in the rebates . I CUT the film so next test will be with my 510-Pyro formula. I was LUCKY we had some SUNSHINE at LAST to test the Contrast. CAMERA was ROLLEIFLEX T with 16-on kit 1/250th @ f6.3 with x2 Yellow Filter - did not do anything to photo!
Pyrocat HD 04
TESTS of KENTMERE 400 120 size in home-made PYROCAT HD Staining Developer . I rated film 320 ASA and gave 17 mins @ 20oC -- there seems to be a High FOG LEVEL in the rebates . I CUT the film so next test will be with my 510-Pyro formula. I was LUCKY we had some SUNSHINE at LAST to test the Contrast. CAMERA was ROLLEIFLEX T with 16-on kit 1/250th @ f6.3 with x2 Yellow Filter - did not do anything to photo!