Back to photostream

Ole No Moire_yellow layer

- 3 min. exposure UV

- 1.5 ml dichromate, 1.0 ml gum arabic

- development 20 minutes only with slight rinse, whoops I was bit too hurry in this.

 

Yellow sticked to the print pretty well. I noticed that the Original print of Ole no moire is not comparable, because of differing color palette. But it will give you guidelines.

348 views
0 faves
1 comment
Uploaded on August 31, 2010
Taken on August 31, 2010