socketball
Stonemask Test Comp
The white is from spill-over on casting the connector pegs in a second pass - I left it that way to see how the overspill works.
Generally successful, some small kinks to work out.
This cast has taught me two things:
1. The new plastic I'm using holds dye much better than the previous stuff. I doubt I'll have to worry about casts getting soft with whatever dye I add.
2. The new plastic is so thin in liquid form that I don't really need to worry about overflow ruining the texture as much as it did with what I was using before. I might even be able to use it to create special effects somehow.
More info on Tumblr.
Stonemask Test Comp
The white is from spill-over on casting the connector pegs in a second pass - I left it that way to see how the overspill works.
Generally successful, some small kinks to work out.
This cast has taught me two things:
1. The new plastic I'm using holds dye much better than the previous stuff. I doubt I'll have to worry about casts getting soft with whatever dye I add.
2. The new plastic is so thin in liquid form that I don't really need to worry about overflow ruining the texture as much as it did with what I was using before. I might even be able to use it to create special effects somehow.
More info on Tumblr.